Chrome free Zinc Flake Coating For Brake Disc JH-310
 1. Other chemicals such as any kinds of acid, alkali salt can not be mixed into coating, for these can activate Zn & Al plate to aging the coating.
2. Avoid irradiation of sunshine and ultraviolet ray for long time when operating, otherwise it will accelerate aging or polymerization of the coating .
3. It is very important to control the temperature of coating. If the temperature of coating changes when operating, it will effect the viscosity, then effec the coating quatity on workpiece. So the relations among temperature,viscosity and spinning process shoud be controlled well when coating.
4. The viscosity will be different if coating method is different. Choose low data if spray coating,and choose high data if dip spin coating.


We cordially invite you to visit our booth:  4B01
                                                                          

Fair details: 

Fair Dates :

19 – 26 October 2016 (Wed - Wed)

Venue :

Dusseldorf Exhibition Centre

ostfach 10 10 06, D-40001 Dusseldorf Stockum Church Street 61, D-40474

Dusseldorf, Germany

 


Web Site:

http://www.k-online.com/cgi-bin/md_k/lib/pub/tt.cgi/K_2016.html?oid=43753&lang=2&ticket=g_u_e_s_t